Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL Card E54153
Arlon 48571R005 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate  (discontinued **)&l
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif..
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL Card E54153
Arlon 19576R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmAppearance: Red silicone gum on polymer linerThis data represents typical values for the production..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. ..
UL RTI, Mechanical without Impact 200 °C
392 °F
E63753
Arlon 41570R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL Card E54153
Arlon 48576R005 0.0055" (0.140 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specific..
UL RTI, Mechanical without Impact 200 °C
392 °F
Arlon 51571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical..
UL RTI, Mechanical without Impact 200 °C
392 °F
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate..
UL RTI, Mechanical without Impact 200 °C
392 °F
File E54153
Arlon 51866R015E 0.0150" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL card E54153
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL card E54153
Arlon 55579R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production materi..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass clot..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 55579XA028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material an..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
UL RTI, Mechanical without Impact 200 °C
392 °F
File E54153
Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material ..
UL RTI, Mechanical without Impact 200 °C
392 °F
File E54153
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
UL RTI, Mechanical without Impact 200 °C
392 °F
File E54153
Arlon 55989R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
UL RTI, Mechanical without Impact 200 °C
392 °F
File E54153
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate..
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL card E54153
Arlon R34931R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL Car E54153
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place ..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 51141R027 0.0270" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values ..
UL RTI, Mechanical without Impact 200 °C
392 °F
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
UL RTI, Mechanical without Impact 200 °C
392 °F
Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
UL RTI, Mechanical without Impact 200 °C
392 °F
Arlon 55141R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 55586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEAppearance: Red silicone gum and rubber on fiberglass clothThis data ..
UL RTI, Mechanical without Impact 200 °C
392 °F
Arlon CP-414R Silicone Rubber
bulk compound
UL RTI, Mechanical without Impact 200 °C
392 °F
per UL Car E54153
Arlon 44580R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti..
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET
Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use..