Material Notes:
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.593 g/cc
0.05755 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Compound Property
Tensile Strength >= 3.10 MPa
>= 450 psi
Compound Property
Elongation at Break >= 275 %
>= 275 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 15.0 - 20.0 min

@Temperature 121 - 177 °C
0.250 - 0.333 hour

@Temperature 250 - 350 °F
Recommended Cure Cycle
120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Users viewing this material also viewed the following: