Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaslok 7021 Black Impact Grade Phenolic Molding Compound  (discontinued **)

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Impact Grade, Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaslok 7021 Black Impact Grade Phenolic Molding Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of switchgear parts, or where mechanical assembly requires better impact strength.Data provided by Plaslok Corporation.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Apparent Bulk Density 0.480 g/cc
0.0173 lb/in³
ASTM D1895
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Compression; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Flexural Yield Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Compressive Yield Strength 228 MPa
33100 psi
ASTM D695
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 171 °C
340 °F
ASTM D648
UL RTI, Electrical 150 °C
302 °F
1.57 mm
UL RTI, Mechanical with Impact 150 °C
302 °F
1.57 mm
UL RTI, Mechanical without Impact 150 °C
302 °F
1.57 mm
Flammability, UL94 V-0
V-0
3.18 mm
V-0
V-0
3.18mm
Electrical Properties Metric English Comments
Electrical Resistivity 6.00e+9 ohm-cm
6.00e+9 ohm-cm
ASTM D257
Dielectric Constant 4.5
4.5
1MHz; ASTM D150
6.0
6.0
60 Hz; ASTM D150
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Dissipation Factor 0.040
0.040
1 MHz; ASTM D150
0.11
0.11
60 Hz; ASTM D150
Comparative Tracking Index 125 V
125 V
UL 746