| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Addiplast Addinyl B2 Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 71 | 71 | Conditioned; ISO 868 |
| 82 | 82 | ISO 868 | |
| Tensile Strength, Yield | 50.0 MPa | 7250 psi | Conditioned; ISO R 527 |
| 80.0 MPa | 11600 psi | ISO R 527 | |
| Elongation at Yield | 30 % | 30 % | ISO R 527 |
| >= 50 % | >= 50 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 0.900 GPa | 131 ksi | Conditioned; ISO 178 |
| 2.80 GPa | 406 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | ISO 180/1A |
| 16.0 kJ/m² | 7.61 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | NB | NB | ISO 179/IeU |
| NB | NB | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/IeA |
| 1.50 J/cm² | 7.14 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM E831 |
| Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | Conditioned; CEI 60093 |
| 1.00e+14 ohm | 1.00e+14 ohm | CEI 60093 | |
| Dielectric Strength | 25.0 kV/mm | 635 kV/in | Conditioned; CEI 60243-1 |
| 26.0 kV/mm | 660 kV/in | CEI 60243-1 | |
| Comparative Tracking Index | 600 V | 600 V | CEI 60112/Solution A |