| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 70 | 70 | Conditioned; ISO 868 |
| 75 | 75 | ISO 868 | |
| Tensile Strength, Yield | 40.0 MPa | 5800 psi | Conditioned; ISO R 527 |
| 45.0 MPa | 6530 psi | ISO R 527 | |
| Elongation at Yield | 50 % | 50 % | ISO R 527 |
| >= 50 % | >= 50 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 0.600 GPa | 87.0 ksi | Conditioned; ISO 178 |
| 1.70 GPa | 247 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | ISO 180/1A |
| NB | NB | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | NB | NB | ISO 179/IeU |
| NB | NB | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | NB | NB | ISO 179/IeA |
| NB | NB | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM E831 |
| Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | Conditioned; CEI 60093 |
| 1.00e+15 ohm | 1.00e+15 ohm | CEI 60093 | |
| Comparative Tracking Index | 600 V | 600 V | CEI 60112/Solution A |