Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers GA-1057H1-VW1LF PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GA-1057H1-VW1LF PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: Lead free 105° C, flat ribbon cable insulation.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 - 1.44 g/cc
1.40 - 1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 92 - 97
92 - 97
ASTM D2240
Tensile Strength 17.2 MPa
2490 psi
ASTM D412
17.88 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
2593 psi

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
Elongation at Break 250 %
250 %
ASTM D412
222.5 %

@Treatment Temp. 136 °C,
Time 605000 sec
222.5 %

@Treatment Temp. 277 °F,
Time 168 hour
Oven aged
Thermal Properties Metric English Comments
Oxygen Index 28 %
28 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+13 ohm-cm
6.00e+13 ohm-cm