Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 79 | 79 | Conditioned; ISO 868 |
85 | 85 | ISO 868 | |
Tensile Strength, Yield | 60.0 MPa | 8700 psi | Conditioned; ISO R 527 |
90.0 MPa | 13100 psi | ISO R 527 | |
Elongation at Yield | 35 % | 35 % | ISO R 527 |
>= 50 % | >= 50 % | Conditioned; ISO R 527 | |
Modulus of Elasticity | 1.30 GPa | 189 ksi | Conditioned; ISO 178 |
3.05 GPa | 442 ksi | ISO 178 | |
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180/1A |
12.0 kJ/m² | 5.71 ft-lb/in² | Conditioned; ISO 180/1A | |
Charpy Impact Unnotched | NB | NB | ISO 179/IeU |
NB | NB | Conditioned; ISO 179/IeU | |
Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179/IeA |
1.10 J/cm² | 5.23 ft-lb/in² | Conditioned; ISO 179/IeA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM E831 |
Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C | 194 °F | ISO 75-2/AF |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Conditioned; CEI 60093 |
1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | Conditioned; CEI 60093 |
1.00e+15 ohm | 1.00e+15 ohm | CEI 60093 | |
Dielectric Strength | 27.0 kV/mm | 686 kV/in | Conditioned; CEI 60243-1 |
28.0 kV/mm | 711 kV/in | CEI 60243-1 | |
Comparative Tracking Index | 600 V | 600 V | CEI 60112/Solution A |