| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.901 g/cc | 0.901 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0044 - 0.0048 cm/cm | 0.0044 - 0.0048 in/in | Unannealed; ASTM D955 |
| 0.0050 - 0.0055 cm/cm | 0.0050 - 0.0055 in/in | Annealed; ASTM D955 | |
| Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 16.1 MPa | 2340 psi | ASTM D638 |
| Tensile Strength, Yield | 20.3 MPa | 2950 psi | ASTM D638 |
| Elongation at Break | 564 % | 564 % | ASTM D638 |
| Elongation at Yield | 5.6 % | 5.6 % | ASTM D638 |
| Tensile Modulus | 1.04 GPa | 151 ksi | ASTM D638 |
| Flexural Modulus | 1.02 GPa | 148 ksi | ASTM D790A |
| Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | 0°F; ASTM D256A |
| 1.87 J/cm | 3.50 ft-lb/in | 32°F; ASTM D256A | |
| 5.87 J/cm | 11.0 ft-lb/in | 72°F; ASTM D256A | |
| Impact Test | 18.2 J | 13.4 ft-lb | ID Impact @ 5mph, Peak Energy; ASTM D3763-86 |
| 31.6 J | 23.3 ft-lb | ID Impact @ 5mph, Total Energy; ASTM D3763-86 |