| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded |
| Manufacturer | Aclo Compounders |
| Trade Name | Accucomp |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accucomp ABS ABS881L Clear Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | MD; ASTM D955 |
| Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
| Flexural Strength | 60.0 MPa | 8700 psi | ASTM D790 |
| Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
| Izod Impact, Notched | 1.28 J/cm | 2.40 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 87.2 °C | 189 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
UL File #E56070 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | clear; thickness not quantified |