| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792-60T |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 78 | 78 | ASTM D785 |
| Tensile Strength, Ultimate | 26.0 MPa | 3770 psi | ASTM D638-61T |
| Elongation at Break | 32 % | 32 % | ASTM D638-61T |
| Izod Impact, Notched | 3.10 J/cm | 5.81 ft-lb/in | ASTM D256-56 |
| 0.800 J/cm @Temperature -40.0 °C |
1.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 147 °C | 297 °F | Flow temperature, ASTM D569-59 |
| Deflection Temperature at 0.46 MPa (66 psi) | 88.0 °C | 190 °F | ASTM D648-56 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.43 @Frequency 10000 Hz |
3.43 @Frequency 10000 Hz |
ASTM D150-54T |
| 3.46 @Frequency 1000 Hz |
3.46 @Frequency 1000 Hz |
ASTM D150-54T | |
| Dissipation Factor | 0.0043 @Frequency 1000 Hz |
0.0043 @Frequency 1000 Hz |
ASTM D150-54T |
| 0.0205 @Frequency 10000 Hz |
0.0205 @Frequency 10000 Hz |
ASTM D150-54T |