Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Kolon Product List

Category
Acrylic, Extruded Thermoplastic Polyurethane, Elastomer, Polyester Grade Thermoplastic Polyurethane, Elastomer, Ether Grade
Acetal Copolymer, Carbon Fiber Filled Acetal Copolymer, Impact Modified Acetal Copolymer, 10% Glass Fiber Reinforced
Acetal Copolymer, 30% Glass Fiber Reinforced Acetal Copolymer, Unreinforced Acetal Copolymer, Silicone Filled
Acetal Copolymer, Mineral Filled Acetal Copolymer, PTFE Filled Polypropylene, Glass/Mineral Reinforced
Nylon 6, Unreinforced Nylon 6, Unreinforced, Flame Retardant Nylon 6, 30% Glass Fiber Filled
Nylon 6, 40% Glass Fiber Filled Nylon 6, Impact Grade Nylon 66, Unreinforced
Nylon 66, Unreinforced, Flame Retardant Nylon 66, Glass Fiber Filled, Flame Retardant Nylon 66, 20% Carbon Fiber Filled
Nylon 66, 20% Glass Fiber Filled Nylon 66, 30% Glass Fiber Filled Nylon 66, 40% Glass Fiber Filled
Nylon 66, 50% Glass Fiber Filled Nylon 66, Impact Grade Nylon 66, Heat Stabilized
Nylon 66, 30% Mineral Filled Thermoplastic Elastomer, Melt-Processible Rubber Polyester TPE
Polyethylene Terephthalate (PET), 30% Glass Reinforced Polyethylene Terephthalate (PET), 20% Glass Reinforced Polyethylene Terephthalate (PET), 50% Glass Reinforced
PEN-PET Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Polybutylene Terephthalate (PBT), Flame Retardant
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Polybutylene Terephthalate (PBT), Impact Grade Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Polybutylene Terephthalate (PBT), Extrusion Grade Nylon 6, Glass Fiber Filled, Flame Retardant Nylon 6, 20% Glass Fiber Filled
Nylon 6, 50% Glass Fiber Filled Nylon 6, Heat Stabilized
Trade Name
DIAMAT® ELLAS Kocetal®
KOLEFIN® Kopa® KOPEL®
KOPET® NOPLA® SPESIN®
Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Kolon DIAMAT® EG Acrylic, Extruded DIAMAT®
Kolon DIAMAT® EM Acrylic, Extruded DIAMAT®
Kolon DIAMAT® IG Acrylic, General Purpose, Molded DIAMAT®
Kolon ELLAS K-260D Thermoplastic Polyurethane Polyurethane, TP ELLAS
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane Thermoplastic Polyurethane, Elastomer, Polyester Grade ELLAS
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane Thermoplastic Polyurethane, Elastomer, Polyester Grade ELLAS
Kolon ELLAS K-475A Ester Based Thermoplastic Polyurethane Thermoplastic Polyurethane, Elastomer, Polyester Grade ELLAS
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane Polyurethane, TP ELLAS
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane Polyurethane, TP ELLAS
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane Thermoplastic Polyurethane, Elastomer, Polyester Grade ELLAS
Kolon KOCETAL® CF702 Conductive Grade Acetal Resin Acetal Copolymer, Carbon Fiber Filled Kocetal®
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin Acetal (POM) Kocetal®
Kolon KOCETAL® EL304 Toughened Grade Acetal Resin Acetal Copolymer, Impact Modified Kocetal®
Kolon KOCETAL® GF702 G/F Reinforced Acetal Resin Acetal Copolymer, 10% Glass Fiber Reinforced Kocetal®
Kolon KOCETAL® K100 Standard Grade Acetal Resin Acetal Copolymer, Unreinforced Kocetal®
Kolon KOCETAL® K200 Standard Grade Acetal Resin Acetal Copolymer, Unreinforced Kocetal®
Kolon KOCETAL® K300LO Low Odor Acetal Resin Acetal (POM) Kocetal®
Kolon KOCETAL® LW701 Wear Modified Acetal Resin Acetal (POM) Kocetal®
Kolon KOCETAL® MS301 Wear Modified Acetal Resin Acetal (POM) Kocetal®
Kolon KOCETAL® SO301 Wear Modified Acetal Resin Acetal Copolymer, Silicone Filled Kocetal®
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin Acetal (POM) Kocetal®
Kolon KOCETAL® WR701 Wear Modified Acetal Resin Acetal (POM) Kocetal®
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene Polypropylene, Glass/Mineral Reinforced KOLEFIN®
Kolon KOPA® KN126 General Purpose Nylon 6 Nylon 6, Unreinforced Kopa®
Kolon KOPA® KN1322VO Flame Retardant Nylon 6 Nylon 6, Unreinforced, Flame Retardant Kopa®
Kolon KOPA® KN133G33HIBL G/F Reinforced Nylon 6 Nylon 6, 30% Glass Fiber Filled Kopa®
Kolon KOPA® KN136 General Purpose Nylon 6 Nylon 6, Unreinforced Kopa®
Kolon Kopa® KN153G30 Nylon 6 Resin Nylon 6, 30% Glass Fiber Filled Kopa®
Kolon Kopa® KN161 Nylon 6 Resin Nylon 6, Unreinforced Kopa®
Kolon KOPA® KN177N Nylon Extrusion Resin Nylon Kopa®
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 Nylon 66, Unreinforced, Flame Retardant Kopa®
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66 Nylon 66, 40% Glass Fiber Filled Kopa®
Kolon KOPA® KN333HRBL Heat Resistant Nylon 66 Nylon 66, Unreinforced Kopa®
Kolon KOPEL® KP3355 General Purpose TPE Resin Thermoplastic Elastomer, Melt-Processible Rubber KOPEL®
Kolon NOPLA® KE531HC PEN-PET Copolyester PEN-PET NOPLA®
Kolon SPESIN® KP212G15V0BM G/F Reinforced & Flame Retardant PBT Compound Resin Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant SPESIN®
Kolon SPESIN® KP212G30V0HI G/F Reinforced & Flame Retardant PBT Compound Resin Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant SPESIN®
Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant SPESIN®
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin Polybutylene Terephthalate (PBT), Impact Grade SPESIN®
Kolon SPESIN® KP213G15SIBL Glass Fiber Reinforced PBT Compound Resin Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled SPESIN®
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled SPESIN®
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled SPESIN®
Kolon SPESIN® KP270BL General Purpose PBT Compound Resin Polybutylene Terephthalate (PBT) SPESIN®
Kolon SPESIN® KP513G30WBL Multi Reinforced PBT Resin Polybutylene Terephthalate (PBT) SPESIN®
Kolon KOPA® KN133G30 G/F Reinforced Nylon 6 Nylon 6, 30% Glass Fiber Filled Kopa®
Kolon Kopa® KN133HB55 Nylon 6 Resin Nylon 6 Kopa®
Kolon KOPA® KN133HR Heat Resistant Nylon 6 Nylon 6, Heat Stabilized Kopa®
Kolon KOPA® KN163HI High Impact Nylon 6 Nylon 6, Impact Grade Kopa®
Kolon Kopa® KN173MS Nylon 6 Resin Nylon 6 Kopa®
Copyright © lookpolymers.com All Rights Reserved