| Eurotec® Tecodur® PB30 NL PBT, unfilled, natural, high viscosity, extrusion grade |
Polybutylene Terephthalate (PBT), Extrusion Grade |
Tecodur®
|
| Eurotec® Tecodur® PB50 NL PBT, unfilled, natural, high viscosity |
Polybutylene Terephthalate (PBT), Unreinforced, Molded |
Tecodur®
|
| Eurotec® Tecodur® PB7 GR15 NL RT PBT, 15% glass fiber reinforced, PTFE modified, natural |
Polybutylene Terephthalate (PBT), PTFE Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, heat stabilized, black |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 BR20 NL100 HS PBT, 20% glass fiber reinforced, heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black |
Polybutylene Terephthalate (PBT), Carbon Fiber Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GB20 NL PBT, 20% glass bead reinforced, natural |
Polybutylene Terephthalate (PBT), Glass Bead Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural |
Polybutylene Terephthalate (PBT), Glass Bead Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GF45 NL PBT 45% filled, high gloss, increased density |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural |
Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 BK EF PBT, 15% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade |
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 BK002 WX21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 BK002 XA21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 NL TD 28 PBT 15% glass fiber reinforced, UL94 V0, impact modified, high CTI |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 NL XA 20 PBT 15% glass fiber reinforced, UL94 V0 |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 NL100 KA01 PBT/PET, 15% glass fiber reinforced, heat stabilized, natural, gas injection grade |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural |
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black |
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural |
PBT + PET Blend, Glass Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR20 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade |
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR25 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL CA 01 PBT/PET 30% glass fiber reinforced |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL FY 10 PBT 30% glass fiber reinforced, UL94 V2 |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL IL PBT 30% glass fiber reinforced, impact modified |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL MB04 PBT/ASA, 30% glass fiber reinforced, heat & UV stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL SV20 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL XA 20 PBT 30% glass fiber reinforced, UL94 V0 |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0 |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL XA60 PBT, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus, heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural |
Polybutylene Terephthalate (PBT), Heat Resistant |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB70 GR50 NL100 PBT, 50% glass fiber reinforced, natural |
Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 NL IL PBT, impact modified, natural |
Polybutylene Terephthalate (PBT), Impact Grade |
Tecodur®
|
| Eurotec® Tecodur® PB70 NL IM PBT, unfilled, impact modified, natural |
Polybutylene Terephthalate (PBT), Impact Grade |
Tecodur®
|
| Eurotec® Tecodur® PB70 NL PBT, unfilled, natural |
Polybutylene Terephthalate (PBT), Unreinforced, Molded |
Tecodur®
|
| Eurotec® Tecodur® PB70 NL RT PBT, unfilled, PTFE modified, natural |
Polybutylene Terephthalate (PBT), PTFE Filled |
Tecodur®
|
| Eurotec® Tecodur® PB70 NL TD20 PBT, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural |
Polybutylene Terephthalate (PBT), Impact Grade |
Tecodur®
|
| Eurotec® Tecodur® PB70 NL TD22 PBT/PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural |
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced |
Tecodur®
|
| Eurotec® Tecodur® PB70 NL XA 20 PBT unreinforced, UL94 V0 |
Polybutylene Terephthalate (PBT) |
Tecodur®
|
| Eurotec® Tecodur® PB80 NL TD 21 PBT/PC unreinforced, UL94 V0, impact modified |
Polycarbonate (PC) |
Tecodur®
|
| Eurotec® Tecoform® PO20 GR10 NL HS POM, 10% glass fiber reinforced, heat stabilized, natural |
Acetal Copolymer, 10% Glass Fiber Reinforced |
Tecoform®
|
| Eurotec® Tecoform® PO20 GR25 NL HS POM, 25% glass fiber reinforced, heat stabilized, natural |
Acetal Copolymer, 30% Glass Fiber Reinforced |
Tecoform®
|
| Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural |
Acetal Copolymer, Impact Modified |
Tecoform®
|
| Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural |
Acetal Copolymer, PTFE Filled |
Tecoform®
|
| Eurotec® Tecoform® PO30 GB30 NL HS POM, 30% glass bead reinforced, heat stabilized, natural |
Acetal Copolymer, Glass Bead Filled |
Tecoform®
|
| Eurotec® Tecolen® HP10 GR30 NL HS PPCP, 30% glass fiber reinforced, heat stabilized, natural |
Polypropylene with 30% Glass Fiber Filler |
Tecolen®
|
| Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural |
Polypropylene with Glass Fiber + Bead Filler |
Tecolen®
|
| Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural |
Polypropylene, Flame Retardant |
Tecolen®
|
| Eurotec® Tecomid® NA30 GR50 BK002 XA40 PA6.6, 50% glass fiber reinforced, flame retardant, heat stabilized, natural |
Nylon 66, 50% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA30 NL RM PA6.6, MoS2 modified, natural |
Nylon 66, MoS2 Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GB30 NL HS PA6.6, 30% glass bead reinforced, heat stabilized, natural |
Nylon 66, Glass Bead Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural |
Nylon 66, 10% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR15 GR003 XA70 PA6.6, 15% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural |
Nylon 66, 20% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural |
Nylon 66, Heat Stabilized |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR25 GR003 XA70 PA6.6, 25% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035 |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural |
Nylon 66, Heat Stabilized |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR25 NL XA 42 PA 6.6 25% glass fiber reinforced, UL94 V0, red phosphorus |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR25 NL XA60 PA6.6, 25% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL HS PA6.6, 30% glass fiber reinforced, heat stabilized, natural |
Nylon 66, Heat Stabilized |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL HW PA6.6, 30% glass fiber reinforced, hydrolysis stabilized, natural |
Nylon 66, 30% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL IH PA6.6, 30% glass fiber reinforced, impact modified, natural |
Nylon 66, Heat Stabilized |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL RM PA6.6, 30% glass fiber reinforced, MoS2 modified, natural |
Nylon 66, 30% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL RT PA 6.6 30% glass fiber reinforced, very low friction and wear |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural |
Nylon 66, PTFE Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural |
Nylon 66, 40% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR40 NL PA 6.6 40% glass fiber reinforced |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural |
Nylon 66, 40% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural |
Nylon 66, 50% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural |
Nylon 66, 50% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 KG30 NL 0B PA6.6, 30% glass fiber/glass bead reinforced, natural |
Nylon 66, Glass Bead Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 MF40 BK001 HS PA6.6, 40% mineral filled, heat stabilized, black |
Nylon 66, 40% Mineral Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural |
Nylon 66, 20% Mineral Filled |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL E PA 6.6 lubricated, nucleated |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural |
Nylon 66, Unreinforced, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural |
Nylon 66, Impact Grade |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL RM PA 6.6 low friction and wear |
Nylon 66 |
Tecomid®
|
| Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural |
Nylon 66, Unreinforced, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural |
Nylon 66, 60% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NB30 BK EF PA6, unfilled, black, suitable for electrostatic powder coating |
Nylon 6, Unreinforced |
Tecomid®
|
| Eurotec® Tecomid® NB30 GR13 BK EF PA6, 13% glass fiber reinforced, black, suitable for electrostatic powder coating |
Nylon 6, 10% Glass Fiber Filled |
Tecomid®
|
| Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NB40 GB30 NL PA6, 30% glass bead reinforced, natural |
Nylon 6, Glass Bead Filled |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR15 NL XA70 PA6, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR20 NL PA 6 20% glass fiber reinforced |
Nylon 6 |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR20 NL XA 20 PA 6 20% glass fiber reinforced, UL94 V0 |
Nylon 6 |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR20 NL XA60 PA6, 20% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Tecomid®
|
| Eurotec® Tecomid® NB40 GR30 NL IM PA6, 30% glass fiber reinforced, impact modified, natural |
Nylon 6, 30% Glass Fiber Filled |
Tecomid®
|