Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Palm Labs Adhesives TURBO FUSE METHYL FOR METALS (75-95 Viscosity) Rapid Bonding Adhesive Palm Lab's Methyl Cyanoacrylate is a one component rapid bonding adhesive ideal for metal surfaces. TURBO FUSE METHYL’s advanced formula is designed to polymerize instantly by absorbing surface moi.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Manifattura Cattaneo VESPEL® SP1 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® ABS GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PEEK GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Techmer ES Plastiblend® PC/PBT IM 6120 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+16 ohm-cm @Temperature 23.0 °C |
1.00e+16 ohm-cm @Temperature 73.4 °F |
50% RH; ASTM D257 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 93 |
Supreme Petrochem SP 6456 High Heat Polystyrene Characteristics High heat resistance & strength Very good flow properties Available in any dark colorsProcessing Injection moldingApplications Instrument enclosures TV components Electrical encl.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ISO 60695 |
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled Hiprolon® 70 MC HLS G30 polyamide 6.10 compound reinforced with 30% chopped glass fiber for injection molding. Features: high heat resistance, dimension stability, impact resistance, good flow ab.. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC250 |
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | DIN 53482 |
Polyram RamTough PZ300G8 Polycarbonate, 40% Glass Fiber 40% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Volume Resistivity | <= 1.00e+16 ohm-cm | <= 1.00e+16 ohm-cm | ASTM D257 |
Daikin NEOFLON M-300P PCTFE Pellets NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | DIN 53 482, VDE 0303, Part 3 |
Hippe PI Wide temperature range for use. High oxidation resistance. UV stability, low coefficient of linear expansion, good strength at high temperatures, resistance against stress cracking.Information pro.. |
|||
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 60093 |
Eurostar Staramide AG6 PA66, 30% Glass Filled, Injection Molded AG6 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Eurotec® Tecodur® PB70 NL RT PBT, unfilled, PTFE modified, natural Information provided by Eurotec® |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Covestro Bayblend® FR630 GR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Eurotec® Tecodur® PB70 GR20 NL CA 01 PBT/PET 20% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
Barlog Plastics KEBAFORM C 909 WR POM Copolymer unreinforced, UV-stabilized POMInformation provided by BARLOG plastics GmbH. |
|||
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Beijing Chemical Industry KAIFA® S-114 PPS Resin Glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |