Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® ABS GF30 A1 30% Glass Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® ABS GF30 A1 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 96.5 MPa
14000 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ASTM D638
Flexural Strength 128 MPa
18500 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.84 J/cm

@Thickness 3.17 mm
7.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.8 µm/m-°C
16.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
233 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
218 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm