Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | |
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam.. |
|||
Dielectric Strength | 80.0 - 100 kV/mm | 2030 - 2540 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A70 white Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A700 BK VN4255 LS Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A700 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Dielectric Strength | >= 80.0 kV/mm | >= 2030 kV/in | Qualified |
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in .. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PB302G50 Nylon 6, 50% Glass Fiber 50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 internationalInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PA323G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, flame retardant, halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PA325G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PA340S6 Nylon 6.6, 30% Glass beads 30% glass beads reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PA340S8 Nylon 6.6 for Injection Molding, 40% Glass-beads Reinforced 40% Glass-beads reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB300G7 Nylon 6, 35% Glass Fiber 35% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB302G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB302G8 Nylon 6, 40%Glass Fiber 40%glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB305G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized and UV stabilized polyamide 6 approved and listed by W.R.C and NSF/ANSI 61 international for potable waterInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB306G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PB340S4 Nylon 6 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced, Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek RA325J5 Nylon 6.6, 25% Glass beads and Glass Fiber, Flame Retardant 25% glass beads and glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60250 |
Polyram PlusTek PB300G2 Nylon 6 for Injection Molding, 10% Glass-Fiber Reinforced 10% Glass-fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | VDE 0303/4 |
Polyram PlusTek PB310G6 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | ASTM D149, IEC 243 |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Dielectric Strength | >= 80.0 kV/mm | >= 2030 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |