Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.13 g/cc | 0.0408 lb/in³ | ±0.03 g/cm³; DIN 53479 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 60.0 MPa @Temperature 23.0 °C |
8700 psi @Temperature 73.4 °F |
ISO 527-2/50 |
Elongation at Yield | 25 % @Temperature 23.0 °C |
25 % @Temperature 73.4 °F |
ISO 527-2/50 |
Tensile Modulus | 1.60 GPa @Temperature 23.0 °C |
232 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eU | |
Charpy Impact, Notched | 0.840 J/cm² @Temperature -30.0 °C |
4.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
5.30 J/cm² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 261 °C | 502 °F | ISO 3146 |
Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous (GTP 50% Tensile); IEC 60216 |
200 °C | 392 °F | Short Time; IEC 60216 | |
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Unannealed; ISO 75-2/B |
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Unannealed; ISO 75-2/A |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Dielectric Constant | 5.0 @Frequency 1.00e+6 Hz |
5.0 @Frequency 1.00e+6 Hz |
IEC 60250 |
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
Dissipation Factor | 0.20 @Frequency 1.00e+6 Hz |
0.20 @Frequency 1.00e+6 Hz |
IEC 60250 |
Comparative Tracking Index | 600 V | 600 V | Solution A; IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Forms | Pellets | |
Generic Material | Nylon 66 | |
Generic Name | Polyamide 66 (Nylon 66) | |
K-Value | 74.0 to 78.0 | No Standard; 96% H2SO4 |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
RoHS Compliance | RoHS Compliant |