Material Notes:
33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
DIN 53479
Water Absorption 6.6 %
6.6 %
DIN 53495
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM-D785
Tensile Strength, Yield 180 MPa
26100 psi
ASTM-D638
Elongation at Break 3.5 %
3.5 %
ASTM-D638
Flexural Strength 250 MPa
36300 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM-D790
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 217 °C
423 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 80.0 kV/mm
2030 kV/in
VDE 0303/4