Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Plastcom SLOVAMID 6 GF 30 FRG 4 LW PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
Kingfa JH830T Flame Retardant PC Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D145 |
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149/DIN 53481 |
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149/DIN 53481 |
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
Kolon SPESIN® KP270 General Purpose PBT Base Resin Excellent extrudabilityApplications: CablesInformation provided by API-Kolon. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.00 mm |
711 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® T 40 ZS 000000 Partially aromatic polyamide Partially aromatic polyamide, injection molding and extrusion grade, easy release, transparent in all wall thicknesses, isotropic shrinkage, mechanical and electrical properties largely unaffected b.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
Lanxess Pocan® T 7391 000000 PBT + PET, 45% Glass Fiber PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® T 40 000000 Partially aromatic polyamide Partially aromatic polyamide, injection molding and extrusion grade, transparent in all wall thicknesses, isotropic shrinkage, mechanical and electrical properties largely unaffected by conditioning.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243 |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 1010R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
Solvay Specialty Polymers Polidiemme® G/450 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60112 |
Stratasys® ABS-M30 ABS-M30 is 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual prototyping, design verification, and direct digital manufacturing. ABS-M30 has greater tensile,.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
ExxonMobil Vacmul 3 A Vacmul 3 A is a non-staining, low-viscosity mineral oil, intended for use as an EDM fluid or as a light- to moderate-duty honing oil. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Covestro Makroblend® UT-1018 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingSheet extrusionInformation provided by Bayer Polymers.As of 1 .. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |
|||
Dielectric Strength | >= 28.0 kV/mm | >= 711 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
SYNTHOS Krasten® 336M High Impact Polystyrene Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos. |