| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET) |
| Manufacturer | Lanxess |
| Trade Name | Pocan® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Lanxess Pocan® T 7391 000000 PBT + PET, 45% Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
| Water Absorption | 0.30 % | 0.30 % | Test Sim. to ISO 62 |
| Moisture Absorption at Equilibrium | 0.10 % | 0.10 % | 23°C/50% R.H.; Test Sim. to ISO 62 |
| Viscosity Test | 80 cm³/g | 80 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
| Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 260 °C |
42 g/10 min @Load 11.0 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 165 MPa | 23900 psi | ISO 527-1/-2 |
| Elongation at Break | 1.7 % | 1.7 % | ISO 527-1/-2 |
| Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA | |
| Impact | 775 | 775 | Puncture maximum force (N); ISO 6603-2 |
| Puncture Energy | 3.50 J | 2.58 ft-lb | ISO 6603-2 |
| Tensile Creep Modulus, 1 hour | 16500 MPa | 2.39e+6 psi | ISO 899-1 |
| Tensile Creep Modulus, 1000 hours | 15000 MPa | 2.18e+6 psi | ISO 899-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 225 - 250 °C | 437 - 482 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 225 °C | 437 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 150 °C | 302 °F | ISO 75-1/-2 |
| Vicat Softening Point | 210 °C | 410 °F | 50°C/h 50N; ISO 306 |
| Flammability, UL94 | HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
IEC 60695-11-10 |
| HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
IEC 60695-11-10 | |
| Oxygen Index | 21 % | 21 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 4.2 @Frequency 1.00e+6 Hz |
4.2 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 4.3 @Frequency 100 Hz |
4.3 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.0020 @Frequency 100 Hz |
0.0020 @Frequency 100 Hz |
IEC 60250 |
| 0.014 @Frequency 1.00e+6 Hz |
0.014 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 275 V | 275 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 270 °C | 518 °F | Injection Molding; ISO 294 |
| Mold Temperature | 90.0 °C | 194 °F | Injection Molding; ISO 10724 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additives | Release agent | |
| Features | Heat stabilized or stable to heat | |
| Form | Pellets | |
| ISO Shortname | ISO 7792-1-PBT+PET,GHMR,09-160,GF45 | |
| Processing | Injection molding | |
| Region | Asia Pacific | |
| Europe | ||
| Near East/Africa | ||
| North America | ||
| South and Central America |