Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.0 kV/mm | 660 kV/in | |
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | |
Plastcom SLOVALEN PH 96 FRD 1 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243-1 |
DSM Arnite® TV4 460 KL TV4 460 PBT/PET Blend-30% Glass Reinforced (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
660 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
660 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 26.0 - 49.0 kV/mm | 660 - 1240 kV/in | Average value: 37.2 kV/mm Grade Count:8 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.00 mm |
660 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Dielectric Strength | 26.0 kV/mm | 661 kV/in | ASTM D149 |
Multibase Multi-Flamâ„¢ 0803 LDPE NH Yellow Polyethylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm |
660 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Asia Pacific) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | CEI 93 |
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA66, Eh 50 TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Properties: High F.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 NATURAL FA PA66, Conditioned Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Dielectric Strength | >= 26.0 kV/mm | >= 660 kV/in | |
Dow Corning SE 4402 KIT One-part, grey, heat cure, good flowability, thermally conductive, controlled volatility.Information provided by Dow Corning |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | ASTM D149 |
Entec Hylox® 9015 PBT, 15% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | |
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | CEI 60243-1 |
Addiplast Addinyl B2 E Flame Retardant Nylon 6 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | |
Arkema Group Rilsan® BECN P20 TL Nylon 11 (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm |
660 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm |
660 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® MN301-G10 Nylon 66 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | ASTM D149/DIN 53481 |
Kolon SPELLOY® KB133G30 PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | Conditioned; IEC 60243 |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |
|||
Dielectric Strength | 26.0 kV/mm | 660 kV/in | CEI 60243-1 |
Addiplast Addinyl B2 Nylon 6 Unreinforced, medium viscosityInformation provided by Addiplast. |