| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Dow Corning SE 4402 KIT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.16 g/cc <br>@Temperature 25.0 °C |
2.16 g/cc <br>@Temperature 77.0 °F |
|
| Viscosity | 34000 cP | 34000 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 74 | 74 | |
| Tensile Strength, Ultimate | 6.10 MPa | 885 psi | |
| Elongation at Break | 120 % | 120 % | |
| Shear Strength | 3.34 MPa | 485 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.920 W/m-K | 6.38 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 200 °C | 392 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
| Dielectric Constant | 4.8 <br>@Frequency 1.00e+6 Hz |
4.8 <br>@Frequency 1.00e+6 Hz |
|
| Dielectric Strength | >= 26.0 kV/mm | >= 660 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 30.0 min <br>@Temperature 150 °C |
0.500 hour <br>@Temperature 302 °F |
|
| Shelf Life | 6.00 Month | 6.00 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | grey | |
| Flowable | yes | |
| Hydrophobic | yes | |
| Self Leveling | yes | |
| Water Resistant | yes |