| Category | Polymer , Thermoplastic , Polyethylene (PE) , LDPE |
| Manufacturer | Multibase |
| Trade Name | Multi-Flam™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Multibase Multi-Flamâ„¢ 0803 LDPE NH Yellow Polyethylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
| Water Absorption | 0.020 % | 0.020 % | at Equilibrium; ASTM D570 |
| Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
| Melt Flow | 1.37 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.37 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 88 | 88 | ASTM D2240 |
| Tensile Strength, Ultimate | 8.07 MPa | 1170 psi | ASTM D638 |
| Elongation at Break | 1000 % | 1000 % | ASTM D638 |
| Flexural Strength | 5.17 MPa | 750 psi | ASTM D790 |
| Flexural Modulus | 0.185 GPa | 26.8 ksi | Method I (3 point load), Procedure B); ASTM D790 |
| Izod Impact, Notched | 3.84 J/cm | 7.20 ft-lb/in | 73°F; ASTM D256 |
| Gardner Impact | 14.35 J | 10.58 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | V-0 | V-0 | 0.0866 in |
| V-0 | V-0 | 0.125 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.80e+15 ohm-cm | 1.80e+15 ohm-cm | ASTM D257 |
| Dielectric Constant | 2.64 @Frequency 100000 Hz |
2.64 @Frequency 100000 Hz |
ASTM D150 |
| 3.15 @Frequency 100 Hz |
3.15 @Frequency 100 Hz |
ASTM D150 | |
| Dielectric Strength | 26.0 kV/mm | 661 kV/in | ASTM D149 |
| Dissipation Factor | 0.015 @Frequency 100000 Hz |
0.015 @Frequency 100000 Hz |
ASTM D150 |
| 0.016 @Frequency 100 Hz |
0.016 @Frequency 100 Hz |
ASTM D150 |