Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It .. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Dielectric Strength | 21.0 - 60.0 kV/mm | 533 - 1520 kV/in | Average value: 31.3 kV/mm Grade Count:20 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PET+PTFE Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149/DIN 53481 |
Kolon KOPA® KN133G33HIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.00 mm |
533 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.00 mm |
533 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66 EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66 High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149/DIN 53481 |
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.91 mm |
533 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | |
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.59 mm |
533 kV/in @Thickness 0.0625 in |
Perpendicular, Short Time in Oil and Air; ASTM D149 |
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and t.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Samyang Tramid® 210G25 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G25 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | ASTM D149 |
Samyang Tribit® 1500G10 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G10 is a reinforced, general purpose gr.. |
|||
Dielectric Strength | >= 21.0 kV/mm | >= 533 kV/in | ASTM D149 |
Unitika UM-8400-20 Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | IEC 60243-1 |
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSG-35 PA666-GF35 Information provided by EMS Grivory |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35 Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Dielectric Strength | 21.0 kV/mm | 533 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35 Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® HN201-G0 PA6 Resin Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 1.60 mm |
533 kV/in @Thickness 0.0630 in |
Short Term; ASTM D149 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Dielectric Strength | 21.0 kV/mm @Thickness 2.00 mm |
533 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LARAMID G/50 50% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |