Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Kolon
Trade Name Kopa®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.40 %
0.40 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength 181 MPa
26300 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Strength 284 MPa
41200 psi
ASTM D790
Flexural Modulus 8.63 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C
11.1 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 247 °C
477 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.6
3.6
ASTM D150
Dielectric Strength 21.0 kV/mm
533 kV/in
ASTM D149
Arc Resistance 135 sec
135 sec
ASTM D495