Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.0 kV/mm | 483 kV/in | |
Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Dielectric Strength | 19.0 kV/mm @Frequency 100 Hz |
483 kV/in @Frequency 100 Hz |
|
Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | |
Pyrotek TS-107 Thermoset Electrical Insulation Product (Nema Grade: G-7) Glass reinforcement, Silicone resin, White color. High temperature resistance. Good electrical properties in humidity.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulato.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 243/1 |
Gharda Chemicals GATONE™ 5300 PEEK, High Viscosity Grade
(discontinued **) High viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical propert.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.00 mm |
483 kV/in @Thickness 0.118 in |
ASTM D149 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Gharda Chemicals Gafone S S1430SP60 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | 1.6mm; ASTM D149 |
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | 1.6mm; ASTM D149 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | 1.6mm; ASTM D149 |
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | 120°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® K300EW Standard Grade Acetal Resin General injection molding grade, toughness is slightly improved. Applications: General injection molding products.Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 1.00 mm |
483 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID GP1300AP PA6, Plasticized Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | VDE 0303 |
GEHR Plastics PEEK Polyetheretherketone Polyether etherketone can be used at very high temperatures and it shows good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical re.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
UBE UPIMOL® S High Heat Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 672-1 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duracon® M450-44/M450S Acetal Co-polymer (POM), Standard, Super high flow, High cycle DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duranex® 751SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Tepcon M450 Acetal-copolymer (POM), Super High Fluidity, High Cycle Information provided by PolyPlastics. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM-D149 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G0 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G0 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duracon® M25-44/M25S Acetal Co-polymer (POM), Standard, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |