Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycolac® MGABS02 ABS General purpose ABS. Excellent flow/impact. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS (Asia Pacific) PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 6.60 mm |
>= 120 arcs @Thickness 0.260 in |
UL 746 |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | PLC 0 |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL Rating PLC 0 (>120 arcs) |
LG Chemical 65IH HIPS High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Asia Pacific) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® 451E PBT 20% GR. Easy flow version of VALOX 451. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL Rating PLC 0 (>120 arcs) |
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL Rating PLC 0 (>120 arcs) |
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | |
DuPont Teijin Films Mylar® EL21 Polyester Film, 900 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |