Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® FXS610SK ABS (Europe-Africa-Middle East) CYCOLAC FXS610SK is a multi purpose ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC FXS610SK is suitable for those applications that require sparkle c.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East) CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East) CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 2.1%); ASTM-D149 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.00 mm |
457 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |