Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 117 sec Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Average value: 150 sec Grade Count:4 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Arc Resistance | 80.0 - 180 sec | 80.0 - 180 sec | Average value: 103 sec Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 121 sec Grade Count:4 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | UL Rating PLC 5 (120-180 sec) |
LG Chemical 20HRI GPPS Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | UL Rating PLC 5 (120-180 sec) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific) Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 1100F PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June 2007, this grade will no longer be supported with biocompati.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 3452 PEI 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 3452 PEI (Asia Pacific) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Arc Resistance | 120 - 180 sec @Thickness 3.00 mm |
120 - 180 sec @Thickness 0.118 in |
UL Rating PLC 5 (120-180 sec) |
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |