| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 80.0 - 130 sec | 80.0 - 130 sec | Average value: 112 sec Grade Count:3 |
|
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Arc Resistance | 80.0 - 180 sec | 80.0 - 180 sec | Average value: 103 sec Grade Count:3 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
|
|||
| Arc Resistance | 80.0 - 85.0 sec | 80.0 - 85.0 sec | Average value: 82.3 sec Grade Count:7 |
|
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
|
|||
| Arc Resistance | 80.0 - 132 sec | 80.0 - 132 sec | Average value: 118 sec Grade Count:5 |
|
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
|
|||
| Arc Resistance | 80.0 - 130 sec | 80.0 - 130 sec | Average value: 119 sec Grade Count:9 |
|
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
|
|||