Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Arc Resistance | 140 - 180 sec | 140 - 180 sec | Average value: 147 sec Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol.. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded
(discontinued **) This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch.. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a .. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for .. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p.. |
|||
Arc Resistance | >= 140 sec | >= 140 sec | ASTM D495 |
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Kolon KOPA® KN333C22 CF Reinforced Nylon 66 Carbon 22%, high strengthApplications Cylinder piston partsInformation provided by API-Kolon. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Haysite 43000 Polyester SMC, 22% Glass Reinforced The 43000 series sheet molding compound is a general purpose material. Designed for compression molding, this grade exhibits good mechanical properties and resistance to mild corrosive agents. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Haysite 46000 Polyester SMC, 30% Glass Reinforced The 46000 series sheet molding compound is designed for "automotive type" applications requiring good mechanical properties and low shrink characteristics. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D-495 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Arc Resistance | 140 sec | 140 sec | Tungsten; ASTM D495 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Arc Resistance | 140 sec | 140 sec | Tungsten; ASTM D495 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Plenco 7080 Phenolic, Nodular, Compression Molded PLENCO 07080 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties along with outstanding resistance to cracking and degradation from soap and de.. |
|||
Arc Resistance | 140 sec | 140 sec | IPC TM-650 2.5.1 |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
Arc Resistance | 140 sec | 140 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.Information provided by Vyncolit, a Sumitomo Bak Group |