Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Mar-Bal
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.90 g/cc
1.70 - 1.90 g/cc
ASTM D792
Bulk Factor 3.0
3.0
ASTM D1895
Filler Content 25 %
25 %
Glass
Water Absorption 0.13 %

@Time 86400 sec
0.13 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cm
0.00050 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 55
45 - 55
ASTM D2583
Tensile Strength 55.2 - 68.9 MPa
8000 - 10000 psi
ASTM D638
Flexural Strength 131 - 152 MPa
19000 - 22000 psi
ASTM D790
Flexural Modulus 11.0 - 11.7 GPa
1600 - 1700 ksi
ASTM D790
Compressive Strength 138 - 165 MPa
20000 - 24000 psi
ASTM D695
Shear Strength 48.3 - 62.1 MPa
7000 - 9000 psi
ASTM D732
Izod Impact, Notched 3.74 - 5.34 J/cm
7.00 - 10.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 14.0 kV/mm
355 kV/in
ASTM D149
Arc Resistance >= 140 sec
>= 140 sec
ASTM D495
Track Resistance 3000 sec
3000 sec
Inclined-Plane Tracking; ASTM D2303
Descriptive Properties Value Comments
Listed File E80533 No
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved