Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | PLC code 0; UL 746A |
SABIC Innovative Plastics Cycolac® X37 ABS ABS, injection moulding, high heat grade.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | 600 V | 600 V | CTI-M 100; IEC 112 |
Nilit FRIANYL A63 RV0 9005 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
DSM Akulon® S223-E Nylon 66 (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V | 600 V | |
LyondellBasell Lupolen® 5361 A HDPE, Blow Molding Grade Easy-to-process blow molding grade for stackable canisters (up to 60 l), used for packing surface-active liquids, laundry and dishwashing detergents, disinfectants, drums (up to 220 l) for various s.. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Comparative Tracking Index | 600 V | 600 V | |
Ineos ABS Lustran® H701 Medium heat resistance, high impact strength. ,Property data per ISO test methods. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | Solution A; IEC 60112 |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Comparative Tracking Index | 600 V | 600 V | UL 746 |
Teknor Apex Chemlon® 143 G Nylon 66, 43% Short Glass Fiber Reinforced Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 112 |
Solvay Technyl® A 205F Nylon 66, EH50 Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula.. |
|||
Comparative Tracking Index | 600 V | 600 V | ASTM D3638 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Comparative Tracking Index | 600 V | 600 V | TS EN 60112 |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Comparative Tracking Index | 600 V | 600 V | dry; IEC 60112 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Comparative Tracking Index | 600 V | 600 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Comparative Tracking Index | 600 V | 600 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® TSS/4 PA666 Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas.. |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 600 V | 600 V | M; IEC 60112 |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 600 V | 600 V | |
BASF Novolen® 1040 N Polypropylene Nucleated grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
ASTM D3638 |
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin 15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Comparative Tracking Index | 600 V | 600 V | |
Arkema Group Orgalloy® LT 5050 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | CEI 60112/Solution A |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Comparative Tracking Index | 600 V | 600 V | CEI 60112/Solution A |
Addiplast Addinyl A2 Nylon 66 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Comparative Tracking Index | 600 V | 600 V | |
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, Dry as Molded
(discontinued **) Injection molding grade, higher stiffness, good stress corrosion cracking resistance and chemical resistance (fuel, cleaning agents).Information provided by Bayer.LANXESS was spun-off from Bayer in .. |