Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific) 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Comparative Tracking Index | <= 100 V | <= 100 V | IEC 112 |
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Comparative Tracking Index | 100 - 600 V | 100 - 600 V | Average value: 420 V Grade Count:54 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM 2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2210 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM MD131A PEI Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics Valox® 508 PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 1212-2 6.4 |
Hippe EP CP 201 Cellulose Paper Reinforced Epoxy Resin - Sheet Used in electronic applications. Good stability of electrical properties under high humidity. Flame retardant.Information provided by Hippe. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 1212-2 6.4 |
Hippe PF CP 205 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions. Flame retardant.Information provided .. |
|||
Comparative Tracking Index | 100 V | 100 V | Test Liquid A; IEC 60112 |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 1212-2 6.4 |
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |