| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
| Water Absorption | 0.060 % <br>@Time 86400 sec |
0.060 % <br>@Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm <br>@Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in <br>@Thickness 0.0591 - 0.126 in |
SABIC Method |
| 0.0050 - 0.0080 cm/cm <br>@Thickness 3.20 - 4.60 mm |
0.0050 - 0.0080 in/in <br>@Thickness 0.126 - 0.181 in |
SABIC Method | |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm <br>@Thickness 1.50 - 3.20 mm |
0.0040 - 0.0060 in/in <br>@Thickness 0.0591 - 0.126 in |
SABIC Method |
| 0.0060 - 0.0090 cm/cm <br>@Thickness 3.20 - 4.60 mm |
0.0060 - 0.0090 in/in <br>@Thickness 0.126 - 0.181 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 119 | 119 | ASTM D785 |
| Tensile Strength at Break | 110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 |
| Flexural Strength | 189 MPa | 27400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 6.89 GPa | 999 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
| 0.800 J/cm <br>@Temperature -30.0 °C |
1.50 ft-lb/in <br>@Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D4812 |
| Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| 8.00 J <br>@Temperature 23.0 °C |
5.90 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 16.2 µm/m-°C <br>@Temperature 60.0 - 138 °C |
9.00 µin/in-°F <br>@Temperature 140 - 280 °F |
ASTM E 831 |
| 23.4 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
13.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 215 °C <br>@Thickness 6.40 mm |
419 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 176 °C <br>@Thickness 6.40 mm |
349 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 |
| UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
| UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
| UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
| Flammability, UL94 | HB <br>@Thickness 1.47 mm |
HB <br>@Thickness 0.0579 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 5.90e+16 ohm-cm | 5.90e+16 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.6 <br>@Frequency 100 Hz |
3.6 <br>@Frequency 100 Hz |
ASTM D150 |
| 3.6 <br>@Frequency 1.00e+6 Hz |
3.6 <br>@Frequency 1.00e+6 Hz |
ASTM D150 | |
| Dielectric Strength | 23.6 kV/mm <br>@Thickness 3.20 mm |
599 kV/in <br>@Thickness 0.126 in |
in air; ASTM D149 |
| 29.1 kV/mm <br>@Thickness 1.60 mm |
739 kV/in <br>@Thickness 0.0630 in |
in oil; ASTM D149 | |
| Dissipation Factor | 0.0014 <br>@Frequency 100 Hz |
0.0014 <br>@Frequency 100 Hz |
ASTM D150 |
| 0.020 <br>@Frequency 1.00e+6 Hz |
0.020 <br>@Frequency 1.00e+6 Hz |
ASTM D150 | |
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
| High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80.0 mm/min | 1.00 - 3.15 in/min | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Specific Volume | 0.66cm^3/g | ASTM D792 |
| UV-light, water exposure/immersion | F2 | UL 746C |