| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | 1 volt; ASTM D4496 |
|
Omni Plastics OmniTech™ CPP XE72-A BK17 ESD Polypropylene Conductive
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
|
|||
| Surface Resistance | 1000 - 1.00e+15 ohm | 1000 - 1.00e+15 ohm | Average value: 4.02e+14 ohm Grade Count:5 |
|
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
PolyOne Stat-Tech™ NY-20CF/000 BLACK Polyamide 6 (Nylon 6)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | ISO D-257 |
|
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **)
PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis..
|
|||
| Surface Resistance | 1000 - 1.00e+18 ohm | 1000 - 1.00e+18 ohm | Average value: 4.11e+16 ohm Grade Count:31 |
|
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 20-8171 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
|
Lehmann & Voss LUVOCOM® 1850-7487 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | ASTM D257 |
|
Techmer ES Electrablend® PA6/6 IM C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Additive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided by TP..
|
|||
| Surface Resistance | 1000 - 10000 ohm | 1000 - 10000 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON RX04031 PA 66 (Europe-Africa-Middle East)
LNP* STARFLAM* RX04031 is a compound based on PA66 resin containing Carbon Fiber, Glass Fiber, Flame Retardant. Added features include: Non-Brominated & Non-Chlorinated Flame Retardant, Electricall..
|
|||
| Surface Resistance | 1000 - 10000 ohm | 1000 - 10000 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP THERMOCOMP DX99077 PC (Europe-Africa-Middle East)
LNP* Thermocomp* DX99077 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Non-..
|
|||
| Surface Resistance | 1000 ohm | 1000 ohm | ASTM D257 |
|
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI
LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding.
|
|||
| Surface Resistance | 1000 - 1.00e+8 ohm | 1000 - 1.00e+8 ohm | ASTM D257 |
|
Techmer ES Electrablend® PA6/6 03003 CF Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact..
|
|||
| Surface Resistance | 1000 ohm | 1000 ohm | ASTM D257 |
|
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled
Information provided by Adamas, HPM
|
|||
| Surface Resistance | >= 1000 ohm | >= 1000 ohm | IEC 60093 |
|
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
|
|||
| Surface Resistance | 1000 - 1.90e+17 ohm | 1000 - 1.90e+17 ohm | Average value: 1.06e+16 ohm Grade Count:36 |
|
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
|
|||
| Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON PX05047 PA 6 (Europe-Africa-Middle East)
LNP* Stat-kon* PX05047 is a compound based on PA 6 resin containing Carbon Fiber, Proprietary Filler (s). Added features include: Electrically Conductive, High Impact.
|
|||
| Surface Resistance | 1000 ohm | 1000 ohm | IEC 93 |
|
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic
(Unverified Data**)
Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable..
|
|||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | IEC 60093 |
|
CENTROPLAST CENTROLEN PP LF Polypropylene conductive
This material is a low density, easily machined plastic that can be welded and has good surface conductivity. Applications include filter heads and housings, conveyor equipment for flammable liquid..
|
|||