Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
Surface Resistance | 10.0 - 1.00e+16 ohm | 10.0 - 1.00e+16 ohm | Average value: 3.03e+15 ohm Grade Count:184 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 2.33e+15 ohm Grade Count:13 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Surface Resistance | 100 - 1.00e+16 ohm | 100 - 1.00e+16 ohm | Average value: 1.24e+15 ohm Grade Count:22 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | Average value: 6.70e+15 ohm Grade Count:3 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Surface Resistance | 10000 - 1.00e+16 ohm | 10000 - 1.00e+16 ohm | Average value: 3.92e+15 ohm Grade Count:26 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+16 ohm | 1.00e+9 - 1.00e+16 ohm | Average value: 2.84e+15 ohm Grade Count:19 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Surface Resistance | 2000 - 1.00e+16 ohm | 2000 - 1.00e+16 ohm | Average value: 8.84e+14 ohm Grade Count:35 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Surface Resistance | 2.60e+9 - 1.00e+16 ohm | 2.60e+9 - 1.00e+16 ohm | Average value: 1.17e+15 ohm Grade Count:25 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 2.51e+15 ohm Grade Count:4 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 1.30e+15 ohm Grade Count:33 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Surface Resistance | 100 - 1.00e+16 ohm | 100 - 1.00e+16 ohm | Average value: 3.89e+14 ohm Grade Count:42 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+16 ohm | 1.00e+12 - 1.00e+16 ohm | Average value: 1.66e+15 ohm Grade Count:10 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 1.56e+15 ohm Grade Count:19 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 7.47e+14 ohm Grade Count:31 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 1.45e+15 ohm Grade Count:23 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 4.36e+14 ohm Grade Count:23 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 8.14e+14 ohm Grade Count:69 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Surface Resistance | 100 - 1.00e+16 ohm | 100 - 1.00e+16 ohm | Average value: 5.18e+14 ohm Grade Count:35 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Surface Resistance | 1.00e+8 - 1.00e+16 ohm | 1.00e+8 - 1.00e+16 ohm | Average value: 7.50e+15 ohm Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | ASTM D257 |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm @Temperature 23.0 °C |
1.00e+15 - 1.00e+16 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers VESPEL TP-8054 Polyimide DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm @Temperature 23.0 °C |
1.00e+15 - 1.00e+16 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers VESPEL TP-8169 Polyimide DuPont Vespel TP-8169 parts are specified for high-temperature applications. TP-8169 parts offer a unique balance of mechanical and thermal properties for high performance in aggressive environments.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 5.72e+14 ohm Grade Count:40 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | Average value: 5.05e+15 ohm Grade Count:4 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+16 ohm | 1.00e+13 - 1.00e+16 ohm | Average value: 3.34e+15 ohm Grade Count:3 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | Average value: 3.02e+15 ohm Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 2.31e+15 ohm Grade Count:45 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 2.82e+15 ohm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |