| Category | Polymer , Thermoplastic , Polyimide, Thermoplastic |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | VESPEL |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers VESPEL TP-8054 Polyimide.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc <br>@Temperature 23.0 °C |
1.33 g/cc <br>@Temperature 73.4 °F |
ASTM D792 |
| Water Absorption | 0.24 % <br>@Temperature 23.0 °C |
0.24 % <br>@Temperature 73.4 °F |
60%RH,23°C,24h; ASTM D570 |
| 0.34 % <br>@Temperature 23.0 °C |
0.34 % <br>@Temperature 73.4 °F |
50%RH,23°C,24h; ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell E | 47 <br>@Temperature 23.0 °C |
47 <br>@Temperature 73.4 °F |
ASTM D785 |
| Tensile Strength | 58.0 MPa <br>@Temperature 150 °C |
8410 psi <br>@Temperature 302 °F |
ASTM D638 |
| 92.0 MPa <br>@Temperature 23.0 °C |
13300 psi <br>@Temperature 73.4 °F |
ASTM D638 | |
| Elongation at Break | 90 % <br>@Temperature 23.0 °C |
90 % <br>@Temperature 73.4 °F |
ASTM D638 |
| 90 % <br>@Temperature 150 °C |
90 % <br>@Temperature 302 °F |
ASTM D638 | |
| Flexural Strength | 88.0 MPa <br>@Temperature 150 °C |
12800 psi <br>@Temperature 302 °F |
ASTM D790 |
| 137 MPa <br>@Temperature 23.0 °C |
19900 psi <br>@Temperature 73.4 °F |
ASTM D790 | |
| Flexural Modulus | 0.00260 GPa <br>@Temperature 150 °C |
0.377 ksi <br>@Temperature 302 °F |
ASTM D790 |
| 0.00290 GPa <br>@Temperature 23.0 °C |
0.421 ksi <br>@Temperature 73.4 °F |
ASTM D790 | |
| Izod Impact, Notched | 0.900 J/cm <br>@Temperature 23.0 °C |
1.69 ft-lb/in <br>@Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 238 °C | 460 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 - 1.00e+18 ohm-cm <br>@Temperature 23.0 °C |
1.00e+17 - 1.00e+18 ohm-cm <br>@Temperature 73.4 °F |
ASTM D257 |
| Surface Resistance | 1.00e+15 - 1.00e+16 ohm <br>@Temperature 23.0 °C |
1.00e+15 - 1.00e+16 ohm <br>@Temperature 73.4 °F |
ASTM D257 |
| Dielectric Constant | 3.1 <br>@Frequency 1.00e+6 Hz,<br> Temperature 23.0 °C |
3.1 <br>@Frequency 1.00e+6 Hz,<br> Temperature 73.4 °F |
ASTM D150 |
| 3.2 <br>@Frequency 10000 Hz,<br> Temperature 23.0 °C |
3.2 <br>@Frequency 10000 Hz,<br> Temperature 73.4 °F |
ASTM D150 | |
| Dissipation Factor | 0.00090 <br>@Frequency 10000 Hz,<br> Temperature 23.0 °C |
0.00090 <br>@Frequency 10000 Hz,<br> Temperature 73.4 °F |
ASTM D150 |
| 0.0034 <br>@Frequency 1.00e+6 Hz,<br> Temperature 23.0 °C |
0.0034 <br>@Frequency 1.00e+6 Hz,<br> Temperature 73.4 °F |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | |
| Forms | Shapes | |
| Material Status | Current | |
| Region Available - Global | Yes | |
| RoHS Compliance | Contact Manufacturer |