Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 1000 ohm | <= 1000 ohm | ASTM D257 |
PolyOne Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP) Information provided by PolyOne |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | IEC 60093 |
PolyOne Trilliant™ HC HC6200-5001 XR Grey Polyamide 12 (Nylon 12) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PP 1383 PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Surface Resistance | 1000 ohm | 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Surface Resistance | 1000 ohm | 1000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Asia Pacific) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
Surface Resistance | 1000 - 1.00e+17 ohm | 1000 - 1.00e+17 ohm | Average value: 5.23e+15 ohm Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Surface Resistance | 1000 - 1.00e+15 ohm | 1000 - 1.00e+15 ohm | Average value: 4.25e+14 ohm Grade Count:12 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | Voltage < 1 V after 2 min - 500 V; ASTM D 257/DIN 53483 |
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound
(discontinued **) Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 1105-8179 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 50-7644 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/BK Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 1105/XCF/40 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Surface Resistance | <= 1000 ohm | <= 1000 ohm | |
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | Dry; ASTM D257 |
Westlake Plastics Zelux® CN-P Polycarbonate (conductive) Carbon-powder-filled with high flexural strength and good thermal stability to 275F. The CN-P is UL94 V-0 rated at 0.030" and is thermoformable in thinner gauges (0.010"-0.060").Information provide.. |
|||
Surface Resistance | 1000 ohm | 1000 ohm | ASTM D257 |
Adamas Adalon® 703 PTFE, 15% Carbon Fiber Information provided by Adamas, HPM |
|||
Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
Techmer ES Statiblend® PPS GF23 IM BK 23% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 23% Filler by WeightAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided.. |
|||
Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific) LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |