Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX AS003 ABS
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Faradex DS0036IP PC
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX KX88084 POM (Europe-Africa-Middle East)
LNP* Faradex* KX88084 is a compound based on POM resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Faradex ZX93134 PPE+PS (Europe-Africa-Middle East)
LNP* Faradex* ZX93134 is a compound based on PPE+PS Blend resin containing Stainless Steel Fiber and Glass Fiber. Added features include: Electrically Conductive, EMI/RFI Shielding.This data was su..
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East)
LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS (Asia Pacific)
LNP* Stat-kon* AX02747 is a compound based on Acrylonitrile Butadiene Styrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Surface Resistance 1.0 - 1000 ohm
1.0 - 1000 ohm
ASTM D257
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite..
Surface Resistance 1.0 - 1000 ohm
1.0 - 1000 ohm
ASTM D257
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information ..
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D4496
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced
Carbon Fiber Reinforced
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D4496
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon DE008E PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE008E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by SA..
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON OE008A PPS - Branched
LNP* STAT-KON* OE008A is a compound based on PPS - Branched resin containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon ZX05043 PPE+PS (Europe-Africa-Middle East)
LNP* Stat-kon* ZX05043 is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE, Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK
LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
IEC 60093
Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin
CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica..
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 (Europe-Africa-Middle East)
LNP * THERMOCOMP* QC006 is a compound based on PA610 resin containing Carbon Fiber. Added features include; Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
Techmer ES Electrablend® PA6 04001 BK MB Glass/Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI..
Surface Resistance 1.0 - 1000 ohm
1.0 - 1000 ohm
ASTM D257
Techmer ES Electrablend® PA6/6 03002 CF Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact..
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DX05042 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257
Techmer ES Electrafil® J-1200/CF/10 ABS, 10% Carbon Fiber Reinforced
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257
Techmer ES Electrafil® J-50/CF/40 Polycarbonate, 40% Carbon Fiber Reinforced, PTFE Lubricated
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66
LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific)
LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Surface Resistance 1.0 - 1000 ohm
1.0 - 1000 ohm
ASTM D257
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.