| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
| Water Absorption | 0.70 % | 0.70 % | 24 hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0010 cm/cm <br>@Thickness 3.17 mm |
0.0010 in/in <br>@Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 248 MPa | 36000 psi | ASTM D638 |
| Elongation at Break | 2.0 % | 2.0 % | ASTM D638 |
| Modulus of Elasticity | 20.7 GPa | 3000 ksi | ASTM D638 |
| Flexural Yield Strength | 352 MPa | 51000 psi | ASTM D790 |
| Flexural Modulus | 18.6 GPa | 2700 ksi | ASTM D790 |
| Izod Impact, Notched | 0.801 J/cm <br>@Thickness 3.17 mm |
1.50 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Unnotched | 6.94 J/cm <br>@Thickness 3.17 mm |
13.0 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 14.4 µm/m-°C <br>@Temperature 20.0 °C |
8.00 µin/in-°F <br>@Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 263 °C | 505 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 254 °C | 489 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
| Surface Resistance | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D4496 |
| Shielding Effectiveness | 20 - 30 dB | 20 - 30 dB | 1000 MHz; ES7-83 |