| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon + PTFE Filled |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Electrafil® J-50/CF/40 Polycarbonate, 40% Carbon Fiber Reinforced, PTFE Lubricated.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.38 g/cc | 0.0499 lb/in³ | ASTM D792 |
| Water Absorption | 0.13 % | 0.13 % | 24 hrs. ASTM D570 |
| Linear Mold Shrinkage | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 193 MPa | 28000 psi | ASTM D638 |
| Elongation at Break | 1.6 % | 1.6 % | ASTM D638 |
| Flexural Yield Strength | 241 MPa | 35000 psi | ASTM D790 |
| Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
| Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 146 °C | 295 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
| Surface Resistance | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D257 |