Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm @Temperature 20.0 - 100 °C |
0.0000750 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Electrical Resistivity | 0.0000750 ohm-cm @Temperature 20.0 - 100 °C |
0.0000750 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm @Temperature 20.0 - 100 °C |
0.0000750 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Electrical Resistivity | 0.0000750 ohm-cm @Temperature 20.0 - 100 °C |
0.0000750 ohm-cm @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide prec.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm @Temperature 20.0 °C |
0.0000750 ohm-cm @Temperature 68.0 °F |
|
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | |
Toho Tenax Besfight® MC Type I (12,000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | |
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | |
Toho Tenax Besfight® MC Type I (6000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-26B Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-28B Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-30B Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-28H Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-32 Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Alliance S-26H Samarium Cobalt Magnetic Material |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | |
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000750 ohm-cm | 0.0000750 ohm-cm | RT |
Outokumpu 725LN Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Electrical Resistivity | 0.0000750 ohm-cm @Temperature 20.0 °C |
0.0000750 ohm-cm @Temperature 68.0 °F |
|
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has.. |