Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.40 g/cc | 0.303 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Vickers | 640 | 640 | |
Modulus of Elasticity | 150 GPa | 21800 ksi | |
Flexural Strength | 90.0 - 150 MPa | 13100 - 21800 psi | |
Compressive Strength | 650 MPa | 94300 psi |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.0 µm/m-°C @Temperature 20.0 °C |
5.56 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
CTE, linear, Transverse to Flow | 12.0 µm/m-°C @Temperature 23.0 °C |
6.67 µin/in-°F @Temperature 73.4 °F |
|
Specific Heat Capacity | 0.390 J/g-°C | 0.0932 BTU/lb-°F | |
Thermal Conductivity | 12.0 W/m-K | 83.3 BTU-in/hr-ft²-°F | |
Maximum Service Temperature, Air | 300 °C | 572 °F |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000750 - 0.0000850 ohm-cm | 0.0000750 - 0.0000850 ohm-cm | |
Magnetic Coercive Force, Hc | 9800 Oe | 9800 Oe | |
20000 Oe | 20000 Oe | Intrinsic | |
Magnetic Remanence, Br | 10600 Gauss | 10600 Gauss | |
Magnetic Maximum Energy Product, BH | 26 MGOe | 26 MGOe | |
Curie Temperature | 750 °C | 1380 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Reversible Temp Coef., Bd | -0.03 %/°C | |
Reversible Temp Coef., Hd | +0.23 %/°C | |
Temperature Coefficient, Br | -0.03 %/°C | (20-100°C) |
Temperature Coefficient, Hci | -0.18 %/°C | (20-100°C) |