Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 39 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Indium Corp. Indalloy 39 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.60 g/cc
0.347 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 15.5

@Load 4.00 kg
15.5

@Load 8.82 lb
2mm ball
Tensile Strength at Break 35.9 MPa
5200 psi
Elongation at Break 100 %
100 %
Modulus of Elasticity 0.103 GPa
15.0 ksi
Thermal Properties Metric English Comments
Heat of Fusion 34.7 J/g
14.9 BTU/lb
Specific Heat Capacity 0.151 J/g-°C
0.0361 BTU/lb-°F
Solid
0.167 J/g-°C
0.0399 BTU/lb-°F
Liquid
Thermal Conductivity 13.0 W/m-K

@Temperature 85.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 96.0 °C
205 °F
Eutectic
Solidus 96.0 °C
205 °F
Liquidus 96.0 °C
205 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 52 %
52 %
Lead, Pb 30 %
30 %
Tin, Sn 18 %
18 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000750 ohm-cm
0.0000750 ohm-cm