| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Fittings 210(HS) Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 81 | 81 | ASTM D2240 |
| Tensile Strength, Yield | 49.0 MPa | 7110 psi | Type I, 51 mm/min; ASTM D638 |
| Tensile Modulus | 2.79 GPa | 405 ksi | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
| Flexural Modulus | 2.79 GPa | 405 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 70.6 °C @Thickness 6.35 mm |
159 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 | |
| Flammability, UL94 | V-0 @Thickness 1.57 mm |
V-0 @Thickness 0.0618 in |
WT; UL 94 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 199 - 210 °C | 390 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | NSF 14 | |
| NSF 61 | ||
| NSF Type I | ||
| Features | High Flow | |
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Injection Molding | |
| PVC Cell Classification | 12454 | ASTM D1784 |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Fittings |