Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 343 - 382 °C | 649 - 720 °F | |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 377 - 382 °C | 710 - 720 °F | Average value: 379 °C Grade Count:3 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melt Temperature | 343 - 382 °C | 650 - 720 °F | Molding |
PolyOne Edgetek® RA-20CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 354 - 382 °C | 669 - 720 °F | Stock |
PolyOne Edgetek® ES-15GF/000 RED Polyethersulfone - 15% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 354 - 382 °C | 669 - 720 °F | Stock |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 354 - 382 °C | 669 - 720 °F | Stock |
PolyOne Edgetek® ES-40GF/000 Polyethersulfone - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 354 - 382 °C | 669 - 720 °F | Stock |
PolyOne Stat-Tech™ PI-05CF/000 Polyetherimide - 5% Carbon Fibers - ESD Applications
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 343 - 382 °C | 650 - 720 °F | Molding |
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 354 - 382 °C | 670 - 720 °F | Molding |
PolyOne Lubri-Tech™ PF-30CF/15T Polysulfone, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 360 - 382 °C | 680 - 720 °F | Molding |
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 354 - 382 °C | 670 - 720 °F | Molding |
PolyOne Stat-Tech™ PI-05CF/000 EM Polyetherimide (PEI)
(discontinued **) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 343 - 382 °C | 650 - 720 °F | Molding |
PolyOne Edgetek® PI-20GM-20CF/000 Polyetherimide (PEI), Carbon/Glass Filled
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedCarbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 343 - 382 °C | 650 - 720 °F | Molding |
PolyOne Edgetek® PF-10GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 343 - 382 °C | 650 - 720 °F | Molding |
PolyOne Edgetek® RA-30CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 354 - 382 °C | 670 - 720 °F | Molding |
PolyOne Stat-Tech™ ES-06CF-09GF/000 Polyethersulfone, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 354 - 382 °C | 670 - 720 °F | Molding |
PolyOne Edgetek® ES-30GF/000 PES (Polyethersulfone), 30% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Melt Temperature | 354 - 382 °C | 670 - 720 °F | Molding |
PolyOne Edgetek® ES-06CF-09GF/000 GREEN Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications
&am Data provided by PolyOne. |
|||
Melt Temperature | 354 - 382 °C | 669 - 720 °F | Stock |
PolyOne Edgetek® ES-06CF-09GF/000 RED Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications
& Data provided by PolyOne. |
|||
Melt Temperature | 354 - 382 °C | 669 - 720 °F | Stock |
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 354 - 382 °C | 669 - 720 °F | Stock |
PolyOne Lubri-Tech™ ES-20GF/15T Polyethersulfone - 20% Glass Fiber Reinforced - 15% PTFE Lubricated