Melt Temperature |
171 - 179 °C |
340 - 354 °F |
|
PolyOne Geon™ Vinyl Wire & Cable 1802-xx11FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible A65M0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible A7501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible A8001 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible A8501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible B6DT0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible B7500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible B7501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible C8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible D7500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible D80M0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
177 - 179 °C |
351 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible D9002 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible K85 Natural & Black Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
171 - 179 °C |
340 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible R343AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible C7500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible C75A0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible C8000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible H41276D Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible R125AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
171 - 179 °C |
340 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible R242BE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
171 - 179 °C |
340 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible R312AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible R352AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
171 - 179 °C |
340 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible R356AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
171 - 179 °C |
340 - 354 °F |
|
PolyOne Geon™ Vinyl Flexible R351AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne |
Melt Temperature |
174 - 179 °C |
345 - 354 °F |
|
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |