Category | Polymer , Thermoplastic , Vinyl (PVC) |
Manufacturer | PolyOne Corporation |
Trade Name | Geon™ |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | PolyOne Geon™ Vinyl Flexible R343AE Polyvinyl Chloride, Flexible (PVC, Flexible).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 67 | 67 | 15 sec; ASTM D2240 |
Tensile Strength at Break | 17.1 MPa | 2480 psi | Type IV, 510 mm/min; ASTM D638 |
Elongation at Break | 400 % | 400 % | Type IV, 510 mm/min; ASTM D638 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -35.0 °C | -31.0 °F | ASTM D746 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 171 - 179 °C | 340 - 354 °F | |
188 - 199 °C | 370 - 390 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Additive | Biocide | |
UV Stabilizer | ||
Features | Flame Retardant | |
Oil Resistant | ||
UV Absorbing | ||
Forms | Pellets | |
Generic Material | PVC, Flexible | |
Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
Processing Method | Extrusion | |
Injection Molding | ||
Profile Extrusion | ||
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
North America | ||
South America | ||
Uses | Flooring | |
Profiles |