| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 70 | 70 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 16.7 MPa | 2420 psi | Type IV, 510 mm/min; ASTM D638 |
| Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 400 % | 400 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -42.8 °C | -45.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
| 188 - 199 °C | 370 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Forms | Pellets | |
| Generic Material | PVC+NBR | |
| Generic Name | Polyvinyl Chloride + NBR (PVC+NBR) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Profile Extrusion | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Hose | |
| Profiles | ||
| Tubing |