Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible D80M0 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PolyOne Geon™ Vinyl Flexible D80M0 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
15 sec; ASTM D2240
78
78
ASTM D2240
Tensile Strength at Break 10.3 MPa
1490 psi
510 mm/min; ASTM D638
Tensile Strength 5.72 MPa

@Strain 100 %
830 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 360 %
360 %
510 mm/min; ASTM D638
Tear Strength 47.3 kN/m
270 pli
Die C, 510 mm/min; ASTM D624
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 1.01 GPa
146 ksi
ASTM D1043
0.310 GPa

@Temperature -22.0 °C
45.0 ksi

@Temperature -7.60 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -18.3 °C
-0.940 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 174 - 179 °C
345 - 354 °F
Descriptive Properties Value Comments
Features Low to No Migration
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Appliance Components
Appliances
Gaskets
Users viewing this material also viewed the following: